DSC and FTIR Testing
3-Day Turnaround
Instant Ordering
Sample Plot
For thermosetting resins and plastics a typical plot is displayed below. In this example, a one component heat activated epoxy resin reports a sharp and well defined single curve with an exotherm of 271 Joules/gram as integrated from the area under the curve. The onset temperature of the exothermic reaction was recorded at 132°C and the peak exotherm temperature of the reaction was 154°C.